#ORNL researchers demonstrate new class of #Nickel-#cobalt superalloys for Additive Manufacturing

Researchers at Oak Ridge National Laboratory (ORNL), Oak Ridge, Tennessee, USA, are reported to have demonstrated that a new class of superalloys, made of cobalt and nickel, remains crack-free and defect-resistant in extreme heat, making them conducive for use in metal Additive Manufacturing applications.

Read more at: https://www.metal-am.com/ornl-researchers-demonstrate-new-class-of-superalloys-for-additive-manufacturing/